  1. Bulk, Exchange-Coupled Nitride Magnets

    Amount: $749,276.00

    During Phase I, we have conducted proof-of-principle experiments to fabricate exchange-coupled isotropic permanent magnets with SmFeN-Fe4N compositions employing shock wave consolidation technique. We ...

    STTRPhase II2007Department of Defense Army
  2. Bulk, Exchange-Coupled Nitride Magnets

    Amount: $99,569.00

    The objective of this proposal is to demonstrate the feasibility of producing exchange-coupled magnets with a mixture of Sm2Fe17Nx and alpha double prime-iron nitride powders as starting materials. Ad ...

    STTRPhase I2006Department of Defense Army
  3. Novel Approaches to Fabricate High Flux Density Magnetic Materials

    Amount: $727,115.00

    Advanced Materials Corporation proposes to optimize the process to manufacture soft magnetic materials that are anticipated to be superior to M19 steels both in magnetic induction and in electrical re ...

    SBIRPhase II2005Department of Defense Navy
  4. Light-Weight Nanocrystalline Hydrogen Storage Materials

    Amount: $100,000.00

    75879-Hydrogen storage materials with a large capacity are needed to store, transport, and utilize hydrogen for fuel cells. This project will employ a unique combinatorial technique for rapidly scree ...

    SBIRPhase I2004Department of Energy
  5. Novel Approaches to Fabricate High Flux Density Magnetic Materials

    Amount: $99,198.00

    M19 grade silicon steel is the most commonly used soft magnet for a number of applications such as in the manufature of motors. Advanced Materials Corporation proposes to fabricate new, proprietary ma ...

    SBIRPhase I2004Department of Defense Navy
  6. A Simple Process to Manufacture Grain Aligned Permanent Magnets

    Amount: $750,000.00

    52 A Simple Process to Manufacture Grain Aligned Permanent Magnets--Advanced Materials Corporation, 700 Technology Drive, P.O. Box 2950, Pittsburgh, PA 15230-2950; (412) 268-5649 Mr. Vijay K. Chan ...

    SBIRPhase II1998Department of Energy
  7. A Novel Technique for the Enhancement of Coercivity in High Energy Permanent Magnets

    Amount: $750,000.00

    51 A Novel Technique for the Enhancement of Coercivity in High Energy Permanent Magnets--Advanced Materials Corporation, 700 Technology Drive, P.O. Box 2950, Pittsburgh, PA 15219-3124; (412) 268-56 ...

    SBIRPhase II1998Department of Energy
  8. A Simple Process to Manufacture Grain Aligned Permanent Magnets

    Amount: $74,840.00

    52 A Simple Process to Manufacture Grain Aligned Permanent Magnets--Advanced Materials Corporation, 700 Technology Drive, P.O. Box 2950, Pittsburgh, PA 15230-2950; (412) 268-5649 Mr. Vijay K. Chan ...

    SBIRPhase I1997Department of Energy
  9. A Novel Technique for the Enhancement of Coercivity in High Energy Permanent Magnets

    Amount: $73,130.00

    51 A Novel Technique for the Enhancement of Coercivity in High Energy Permanent Magnets--Advanced Materials Corporation, 700 Technology Drive, P.O. Box 2950, Pittsburgh, PA 15219-3124; (412) 268-56 ...

    SBIRPhase I1997Department of Energy
  10. Apparatus for the Testing of Solid Cryogenic Mechanical Properties

    Amount: $80,000.00

    The proposed effort in Phase I is to identify properties of propellants that solidify at cryogenic temperatures, "cryosolids", that will be tested in Phase Ii and to deliver a detailed design of a cry ...

    SBIRPhase I1996Department of Defense Air Force
US Flag An Official Website of the United States Government